COB setting for Electrolytic & Electroless Gold

Views: 1570

#62945

COB setting for Electrolytic & Electroless Gold | 19 October, 2010

Hi Guys, I have a couple question regarding COB process.

1. Can I do Al wire bonding on electrolytic and electroless gold PCB using same parameters? Some expert telling me electrolytic and electroless should have different setting

2. I am have a board with below process - IR reflow top side -> IR reflow bottom side-> COB Will 2 times IR reflow affect COB bonding process?

Appreciate any kind of feedback from you guys..

reply »

#62976

COB setting for Electrolytic & Electroless Gold | 22 October, 2010

hi 1) just run test batch and pull test wire. Use MIL std to find out your results.

2) again run through and test wire.

reply »