Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Baking boards

Brian Larson

#6442

Baking boards | 13 June, 2000

How long and at what temperature to you bake through-hole boards for moisture? I am getting blow holes after the wave solder. Everything points to the drilling of the board, but I need to prove that it is not moisture.

reply »

track trace and control

ADJUST-A-VAC Vacuum Tweezer for fragile components, wafers, MEMS devices tweezers