Ersa Hotflow 9 specification | 15 July, 2010

We've recently purchased a second hand smt line which contains an Ersa Hotflow 9 reflow oven.We were informed that this oven was capable of handling a lead free process.The oven was manufactured in 2000,and it has come to our attention that it can only handle solders with a melting point of 200c and below.Be grateful for any information/specs etc before i start running any tests.

reply »