Hi guys,

which is good...

AOI inspection before Aqueous wash of Water Soluble Flux processed PCB's or Wash first before AOI?

regards,

reply »

#62028

AOI Inspection Process for WS Flux PCB's | 9 June, 2010

I guess that depends what you're trying to inspect. Are you inspecting solder joints too? If so, I'd wash them first. But that's just me.

reply »


SC

#62124

AOI Inspection Process for WS Flux PCB's | 25 June, 2010

I'd wash them first then AOI. Especially you use the same AOI for WS and no-clean. You certainly will not want any WS flux left inside teh AOI then use the AOI for a NC PCB...