I am just wondering what other people are using as far as gloves when cleaning the dross out of the wave solder pot. We currently are using welding gloves, but the operators say that they are too big and bulky. Does anyone have any suggestions on what type to be using?

reply »

Pete B

#61014

Wave solder cleaning gloves | 3 February, 2010

We use woven Kevlar gloves and gauntlets. Try Ansell or similar manufacturers.

Pete B.

reply »

#61019

Wave solder cleaning gloves | 3 February, 2010

The Ove Glove, Works great and is MUCH less expensive.

reply »

#61040

Wave solder cleaning gloves | 4 February, 2010

We use Hot Mill Gloves, North by Honeywell. Their part number is 51/7146ZJ. I think they work pretty good. We pay about 4.03 per pair.