Conformal Coating Strip with Connectors??? | 26 January, 2010

Are there any MIL-Std approved methods of striping conformal coating without removing connectors?

reply »

#61064

Conformal Coating Strip with Connectors??? | 7 February, 2010

The US military no longer approves repair processes. What coating material are you aiming to remove? Choices for stripping are: * Chemical solvents * Heat * Media

reply »


Lou

#61168

Conformal Coating Strip with Connectors??? | 19 February, 2010

We regularly strip conformal coating for military customers. Connector removal is not required. The type of coating is the biggest factor. Acrylics and silicones are easy and will come off nicely without any other damage. Epoxy and fully cured polyurethanes are extremely difficult and I would sugest removing any fragile components first. Parylene is not even worth the effort, scrap it.