socket PTH reflow soldering | 21 January, 2010

I have tried to solder sockets by reflow machine. but, failed because sockets were deformed after reflow.Has anyone had some advise for me?

reply »

#60894

socket PTH reflow soldering | 22 January, 2010

This socket supplier never expected you to do what you're doing to his/her part. Some materials bear-up under the thermal strain of reflow solder than others. Try different socket materials.

reply »

#60909

socket PTH reflow soldering | 25 January, 2010

Thanks Davf that socket we couldn't change since the customers supply these sockets.we can contro only our process.

reply »

#60960

socket PTH reflow soldering | 28 January, 2010

i agree, with the other fellow, check the data sheet for the part and see what it can handle otherwise hand assemble.