Hi All,

We have a glenbrook x-ray in house, but I am in need of a high resolution x-ray of some failed BGA image sensors.

Does anyone know of a company that does hi-res or 3D x-ray service? We are not getting enough detail to really see what may be going wrong with one of our assemblies.

thanks!

reply »

#60866

BGA x-ray services 3D | 18 January, 2010

Hi,

At Process Sciences we can provide high-res X-ray inspection. You can view some sample images on our website.

Glenn Robertson

www.process-sciences.com

reply »

#60930

BGA x-ray services 3D | 26 January, 2010

You may want to contact YESTech (www.yestechinc.com) and see if they can help you out. If you are in the market to purchase, they have great systems. If you just need to look at a couple samples, they are pretty good about helping people out.

reply »

#60938

BGA x-ray services 3D | 26 January, 2010

A few years ago we sent some samples to Dage for them to analyze on one of their 3D systems.

reply »

#60941

BGA x-ray services 3D | 26 January, 2010

I agree that Dage makes some excellent 3D (CAT) systems, but in our experience a high-resolution 2D system with tilt capability is usually better-suited for inspection of solder joints.

Glenn Robertson

Process Sciences

reply »

#60957

BGA x-ray services 3D | 28 January, 2010

2D with tilt will work. We have found opens on BGA balls with a 2D system tilted at the right angle.