Hi,

Can someone that has done their PCB's Microsectioned tell me "How much Microsection Could Cost"?

Which company does Microsectioning of PCB's?

thanks

reply »

#60701

How Much does Microsectioning Cost? | 18 December, 2009

ACI Technologies, Inc is who we go to for ours. They are good but its not cheap. Expect to pay almost $1000 for one.

Depending on what you need, your bare PCB manufacturer may do this for you for next to nothing. The information they gain from doing the section for you can help their process as well so its a win win.

reply »

#60710

How Much does Microsectioning Cost? | 21 December, 2009

Two other outside labs you can try. Robisan Labatory 6502 E. 21st Street Indianapolis, Indiana 46219 (317) 353-6249 Phone (317) 917-2379 Fax http://www.Robisan.com

The Specialty Lab, Inc. 2515 Terminal Road Dock F Roseville, MN 55113 Phone: 651-635-5925 Fax: 651-635-5927

$ 450 - + 1000 depending on if other testing is needed.