When applying the ECCOBOND E3503-1 thermal adhesive to attach a HB-LED to the slug area of a MCPCB, should the OSP coating on the slug area first be removed? I have heard that OSP coatings have poor adhesion properties so I'm wondering how to do this.

reply »

#60422

OSP adhesion | 12 November, 2009

We have the same concerns about using OSP with adhesives. On the other hand, some suppliers claim their products work with OSP. This have to be handled on a case-by-case basis. How well does OSP transmit heat? It's quite thin.

reply »

#60507

OSP adhesion | 20 November, 2009

Is it possible to use Reactive Nano Technologies solder process?