Asphalt potting | 4 November, 2009

Is anyone using asphalt to pot assemblies? What temperature do you pour it at?

Thanks!

Craig

reply »

#60315

Asphalt potting | 4 November, 2009

What is the advantage of asphalt versus potting compound?

reply »

#60333

Asphalt potting | 5 November, 2009

Other than low cost Im not sure there is any. All the major ballast manufacturers seem to use asphalt. It costs about $500 per ton.