Photonic Soldering | 19 September, 2000

Does Photonic soldering work well with Ceramic substrate PCB's? and can it be used for die?

reply »

Erick Russell

#6245

Re: Photonic Soldering | 20 September, 2000

Yes, some testing of soldering chip capacitors onto ceramic substrates with high temperature paste proved successful. Die attachment can be achieved using this technology as well. The underfill of the die becomes a critical factor in rework potential of your application. Some new materials have claimed to be reworkable, but the cleaning of the area to place a new die down remains a problem.

reply »

#6246

Re: Photonic Soldering | 21 September, 2000

Is this underfill reworability an issue with the underfill material or you rework machine?

reply »

Erick Russell

#6247

Re: Photonic Soldering | 22 September, 2000

It has been an issue with the underfill material. New products on the market claim to be reworkable. This will be very exciting to see in the future.

reply »