Hello,

Does anyone has experience with Certonal FC472 as conformal coating? It looks very simple to use it. I also think that this is the only benefit to use it. But someone in our company think that this is the best solution. On the web you can only find information on acota site.

Thanks in advance.

Mateja

reply »

#60060

certonal | 7 October, 2009

we have several assemblies coated in certonal. Some are even outsourced by adcota. It is basically 3m's 'Scotch guard'. Very easy to use with no masking required.