CSM84 Ball Screw Lubrication

Views: 1847

#59311

CSM84 Ball Screw Lubrication | 16 July, 2009

The manual says (paraphrasing) "If the ball screw needs lubrication, lubricate the ball screw". Not very helpful 8-) The various linear guides all have grease fittings, but I can not find any for the ball screws. Any advice from CSM84 users would be greatly appreciated!

Thanks, Tom

reply »

#59401

CSM84 Ball Screw Lubrication | 29 July, 2009

You could use SHELL ALVANIA GREASE EP2 or other vehicles solid greases