Alternative PCB Material

Views: 4954

#58913

Alternative PCB Material | 27 May, 2009

Hi

Is there an alternative material to fibreglass that can be used for PCBS ? for a specific application I am looking for something that will absorb little or no moisture.

Regards

reply »

#58944

Alternative PCB Material | 29 May, 2009

Ceramic, maybe

reply »

#58971

Alternative PCB Material | 2 June, 2009

Adam,

Look into Rogers materials, draw back to it is Price and lead time of material.

Regards, boardhouse

reply »

#59013

Alternative PCB Material | 6 June, 2009

If the concern is the increased moisture absorption associated with lead-free capable materials, you probably have the most experience with phenolic materials like Isola IS410 or 370HR.

The best move would be to switch to an IPC 4101/99 or /124 material like FR406HR. We've tested these to have moisture absorption rates of less than 0.1%, as opposed to up to .45% seen in phenolic materials.

reply »