wave soldering | 23 January, 2009

Hello, thanks to everyone that reply to my previous question. I have another request: is it possible to solder polyester capacitors (case 2220) with wave soldering process? Thanks! Regards, Stefano

reply »

#57902

wave soldering | 29 January, 2009

Only if it has exposed ends on the end.