Pick errors from Vishay reels | 3 December, 2008

Our UIC Lightning Head is having pick issues with Vishay reels (0402,0603) when the reel are near the end. It occurs ~300-200 pieces before the end of the reel. Pick point was confirmed and is consistent. Has anyone experienced this issue nearing the end of a reel?

reply »

#57485

Pick errors from Vishay reels | 3 December, 2008

We have an ac30l advantis machine with a lighting head for about a year now we place a lot of 0603 parts some from vishay we are not seeing this problem yet

reply »

#57487

Pick errors from Vishay reels | 3 December, 2008

Its mainly on the heavy hitters when the head is sitting over the feeder (Gold) and doing some multiple picks. Again this only seems to happen near the end of a reel. If we splice the reel is it picks perfectly directly after the splice.

reply »

#57490

Pick errors from Vishay reels | 3 December, 2008

Hi,

we also use Advantis machines. Our software have a software option "Auto teach pick up position". This one is made exactly for not perfect feeders or reels. In case you have this option it could help you. you can set it for each part you want.

Regards, Emil

reply »

JAX

#57507

Pick errors from Vishay reels | 4 December, 2008

Check the spring tension on the reel holder. When the reels start running out of parts the spring can provide enough tension to keep the reel from spinning. I have seen this on some of the dual-lane feeders. Tape the spring back to verify. If this is the problem you should be able to get replacements from UIC for free.

reply »

#57531

Pick errors from Vishay reels | 8 December, 2008

> Check the spring tension on the reel holder. When > the reels start running out of parts the spring > can provide enough tension to keep the reel from > spinning. I have seen this on some of the > dual-lane feeders. Tape the spring back to > verify. If this is the problem you should be able > to get replacements from UIC for free.

The next chance we run i will try to confirm. Thanks

reply »

#57541

Pick errors from Vishay reels | 9 December, 2008

I had similar problems with some Chinese 0805 capacitors. Some parts simply won't get out of the paper tape - like they sticked to the bottom paper tape... It happened on two reels, the rest was OK, so I suppose that was some "glitch" on their side...