Underfill 300balls BGA connector

Views: 1737

#56336

Underfill 300balls BGA connector | 4 September, 2008

All, Does anyone have experience with underfill 300balls BGA connector? We have a component with 300balls BGA connector that connectorize with Flex. Customer wants to have an underfill

Questions - Possibility for underfill 300balls BGA connector - Application of an underfill recommended for 300balls BGA connector - Does one normally require an underfill for this components

Thank,

reply »

#56365

Underfill 300balls BGA connector | 5 September, 2008

> All, Does anyone have experience with underfill > 300balls BGA connector? We have a component with > 300balls BGA connector that connectorize with > Flex. Customer wants to have an > underfill > > Questions - Possibility for > underfill 300balls BGA connector - Application > of an underfill recommended for 300balls BGA > connector - Does one normally require an > underfill for this components > > Thank,

Hi,

that sounds very interesting

By connector, you mean socket? What is the material of the connector(socket)? Is it very frigale? how big are the balls(diameter)?

I know only FC or some CSP to need underfil. If you give more information, we could help with something.

reply »

#56377

Underfill 300balls BGA connector | 7 September, 2008

We have BGA connectors on rigid laminate. Points are: * We love BGA connectors for mating mother/daughter boards because they eliminate the wave solder step required for PTH connectors. * BGA connectors are very tricky to assemble, much trickier than BGA. So, environmental testing is absolutly necessary to validate process and assure reliable product. * We'd guess that underfilling a huge connector like this on flex is a bad idea, because it would create a large rigid surface with multiple CTE.

reply »

#56383

Underfill 300balls BGA connector | 8 September, 2008

By connector, you mean socket? Connector use for board to board connection from FCI, MFG P/N: 84500-202

What is the material of the connector(socket)? Is it very frigale? Housing: liquid crystal polymer Solder ball: SnPb 63/37

how big are the balls(diameter)? Solder ball size: 0.76mm Distance between solder ball: 1.27mm (center to center)

reply »