ec

#55655

SMT Adhesive | 24 July, 2008

Hi. I am currently evaluating what adhesive is best to use for printing and lead free application. can anyone please recommend. Thanks!

reply »

#55665

SMT Adhesive | 24 July, 2008

I use loctite 3616 chipbonder for stencil printing and have good results. If using with a shot meter Loctite 3621 has also produced good results.

reply »


ec

#55748

SMT Adhesive | 29 July, 2008

Hi. Thanks for the response. Can you advise who is your supplier? Thanks!

reply »