Datasheet for VIA BGA | 7 July, 2008

Hello, I have some troubles to find datasheets for BGA VIA Tech. I found some datasheets, but the thermal information I can not find this information. Can anybody help me how can I find the thermal information? Thanks...

reply »

#55395

Datasheet for VIA BGA | 7 July, 2008

Part number?

reply »

#55398

Datasheet for VIA BGA | 7 July, 2008

*VIA VN896CE; *VIA VT8237A;

Thanks!

reply »

#55401

Datasheet for VIA BGA | 7 July, 2008

Upon further investigation I'm stumped.

Usually if the data sheets don't have package and processing information in them they've got a package specific document hidden somewhere but I couldn't find one of those either.

I'd check out the "Contact Us" link next for a phone number.

reply »

#55403

Datasheet for VIA BGA | 7 July, 2008

Asking the part manufacturer for this info would require you to give them the type of paste you use, via hole opening, profile.... etc. That's why they don't have this info. Looks like someone is gonna have to do some old fashion engineering work. Welcome to bold new future!

reply »

#55414

Datasheet for VIA BGA | 8 July, 2008

All I ever look at re: thermal stuff is lead finish, max. proc. temp. and dwells anyway. If what you're shootin' at is profiling info., you're right, they don't know jack about my paste.