Just like to know what you guys thoughts regarding mixed alloys. Production run SAC305 and some components are SAC105. So, which profile should you follow. SAC105? or SAC305.

reply »

#55006

Mixed SAC105 and SAC305 | 6 June, 2008

I've got the same scenario. and I followed SAC105.

reply »

#55325

Mixed SAC105 and SAC305 | 2 July, 2008

Why not follow SAC305? you would do so for any other component finish wouldn't you? A component finish of pure Sn would also not call for a pure Sn profile, would it?