I've been told that there boards out there where some components are recessed into the board to save on assembled height. Has anyone heard of this? I can envision making a build up PWB but it would be expensive and I'm not sure how you assemble it without some exotic deposition process.

reply »

#53628

Multilevel PWBs? | 13 February, 2008

They call these embedded components... I've heard of them and read about them, but I haven't seen any yet.

Here is a short article about embedded components in a PCB: http://tinyurl.com/2j6bd8

reply »

#53629

Multilevel PWBs? | 13 February, 2008

Yes, embedded components. They can build decoupling capacitors and terminating resistors into layers of the PC board, and print them very much like copper layers.