Interleaving paper for Immersion Silver PCBs

Views: 2598

#53243

Interleaving paper for Immersion Silver PCBs | 17 January, 2008

All, Can someone help find a source for purchasing interleaving/packaging paper for Immersion Silver boards (sulfur free + ph neutral ..).

Thank you!

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#53245

Interleaving paper for Immersion Silver PCBs | 17 January, 2008

Google => "silver saver" paper

It can be purchased as an industrial product: * corrosionvci.com/corrosion_control_vci_paper.htm * daubertcromwell.com/pdf/silverg.pdf * corrosionprotection.net/corrosion/proddetail.php?prod=silversaver48R * jamesdawson.com/Silver%20Saver.pdf

In our notes, we have a reference to a NPL presentation [npl.co.uk/ei/presentations/storage.pdf] on the results of a study of the effect on solderability of 'silver saver', but the link doesn't seem to work. Chris Hunt at NPL can probably give you a lead on the results.