BGA 0.5mm pitch Ball 0.3mm assembly and soldering.

Views: 2924

#53026

BGA 0.5mm pitch Ball 0.3mm assembly and soldering. | 26 December, 2007

I am looking for suggestion of BGA 0.5mm pitch Ball 0.3mm (BGA 8x8mm)assembly and soldering. Stencil thickness? Stencil reduce? Etc.

reply »

#53035

BGA 0.5mm pitch Ball 0.3mm assembly and soldering. | 27 December, 2007

5 or 6 mil thicjk stencil and no reduction.

reply »

#53047

BGA 0.5mm pitch Ball 0.3mm assembly and soldering. | 28 December, 2007

We agree with Chunks

reply »

#53056

BGA 0.5mm pitch Ball 0.3mm assembly and soldering. | 2 January, 2008

HA-HA-HA... Krikies. What are ya mate? A slavakian?

reply »

#53124

BGA 0.5mm pitch Ball 0.3mm assembly and soldering. | 9 January, 2008

5 mil thick is the max and no reduction

Any question feel free give me a call @ 714-636-6211 or email me Steve@usastencils.com