We have recently acquired a Passaat SMRO-0406 oven. The manual is uninformative for oven settings. Can someone supply us with starting points for conveyor speed, Zone 1 to 4 and 5 to 8 temperature settings please?

Our boards for a product we manufacture are:

8" by 8", FR-4, 1-oz copper, HAL tin 4-layer, inner layers are ground and power distribution planes. densely packed, SOIC, 0805 and VQFP-44 components AIM WS-353 lead-free solder paste

Thank you very much.

Mariss Freimanis Geckodrive Inc.

reply »

#52005

Oven settings | 9 October, 2007

As a starting point, follow the guidance of your paste supplier: http://www.aimsolder.com/tds/WS%20353%20Sn62%20&%20Sn63%20Solder%20Paste.pdf

reply »


RDR

#52019

Oven settings | 10 October, 2007

you could call DIMA and have them give you a starting recommendation OR get a fab and run it through with a thermocouple and adjust from there.

as a start try these.

220 180 180 300 top and bottom belt speed @.4

I do have one of these ovens and this is a real recipe your results may vary however.