I just wonder anyone had the idea of solderability test for through hole by using a wetting balance equipment? I read the jstd002/003 however my feel is now our machine (metronelec st60) is not capable of this test?

reply »

#47316

through hole solderability | 7 February, 2007

The standard Metronelec Menisco ST 60 can not run a dip and look test for PTH parts. It is an optional feature on that machine.

reply »

dphilbrick

#47317

through hole solderability | 7 February, 2007

Tintronics in Huntsville AL can do this. PS I use them all the time for various services. I have no affiliation with them other than being a customer.