As we have vitronics oven(SMR610A) made in december 1997,which has 5 heating And 2 cooling zones. we just want to confirm that is there any possibility of damage oven parts with long run for soldering of lead free components in this model? if anyone knows about the lead free soldering, please give us some suggestions....

reply »

#46178

Lead free vitronics profile | 15 December, 2006

Hi, Hemendra

Recently, We have carried out lead Free Soldering On our 4+1 Panasonic Reflow machine. Results were fine , but its Not Recommended for long Run.

but the machine which you have is 5 zone machine and additional 2 cooling zone too.

Check your Profile , if it withstand below max limits of Specified limit in manual. then there should not be any problem

Hope this info will help U out

Regards Shrikant Borkar Bangalore

reply »

Loco

#46188

Lead free vitronics profile | 15 December, 2006

Its a vitronics, with a little proper maintenance it'll go on forever!