Connector PAD no solder | 26 June, 2006

Through the pads of conncector(50pin) were printed full solder paste, the solder paste of about 2-5 pads follow to bottom of the connector 2-5 pins, the 2-5 pads outside of connector no any tin after reflow. Is this PCB problem?

I can supply failure photo for reference, how to attach?

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#42437

Connector PAD no solder | 27 June, 2006

It sounds like a board issue.

With the current site software, you can not attach pix. You need to post the pix on another site [eg, imageshack, villagephotos, etc] and then post the link here. Or if only a couple of folk are interested, just email the pix to them.

Email me the pix please.

reply »

YQ Deng

#42461

Connector PAD no solder | 28 June, 2006

Dear Davef,

Please told me your Email address, then I send the photos to you. Thanks!

This message was posted Add this forum to your site! Click to learn more. the Electronics Forum @

reply »

#42466

Connector PAD no solder | 28 June, 2006

YQ Deng: Just click on my name next to the Lou Reed likeness in this posting.