Hi Im trying to find a supplier for 30swg HMP solder wire idealy the alloy I want is 93.5Pb, 5Sn, 1.5Ag, 296 to 301 degrees C. Flux cored. 30swg or 0.3mm diamiter.

but the critcal parts are the diameter and the melting point, 300 degrees +-20 degrees.

Ive tried most companies in the UK but will buy from anywhere.

I want about 5kg

anybody know where i can find it?

reply »


RDR

#41534

WANTED: HMP 30swg, (0.3mm) solder wire supplier | 15 May, 2006

Have you tried Indium corp?

reply »


Rob

#41538

WANTED: HMP 30swg, (0.3mm) solder wire supplier | 15 May, 2006

Possibly Warton Metals TLS/5