tsop

Jason

#4816

tsop | 25 February, 2000

Is there any special precautions i should take when removing and replacing 48 pin TSOP'S

reply »

#4817

Re: tsop | 26 February, 2000

Jason: Assuming you wantto reuse the TSOPs, two things come to mind:

1 Don't bend the leads. This can be caused by not melting the solder on all leads at the same time. 2 Don't break the body. This can be caused by moisure absorbed by the case expanding when heated during desoldering.