Local Cleaning Post Rework on PCB with Conformal Coating

Views: 1246

#66090

Local Cleaning Post Rework on PCB with Conformal Coating | 2 April, 2012

Wondering how you guys do this.

Scenario: You have to rework a part (small IC or resistor) on a board that has already been conformal coated with acrylic.

What do you do with the post soldering residues before you cover it up with fresh coating? I know what we do, and I have never felt comfortable with the local clean and blot method.

I was wondering if a small vacuum existed, kind of like at the dentist office that could clean and vacuum at the same time? If not, i know what my next project will be!

Thanks,
JD

reply »

#66092

Local Cleaning Post Rework on PCB with Conformal Coating | 2 April, 2012

The way you phrased the question implies that your rework uses OA. Why not do low res rework?

reply »

#66093

Local Cleaning Post Rework on PCB with Conformal Coating | 2 April, 2012

Hi Dave, we certainly do use low res. Still not comfortable with leaving anything behind however...Figured some brain would have a product for this.

If not, this brain will have to create one and sell to other brains on this forum.

:)

reply »

#66154

Local Cleaning Post Rework on PCB with Conformal Coating | 13 April, 2012

We actually have a product on the dwg bd for this.

Contact me off line if interested.