We are facing the problem of dry soldering in chip capacitor... - Nov 21, 2005 by MSK
It sounds like you're exhausing your flux activity on this c... - Nov 22, 2005 by davef
Thanx for your only reply!! I already increased temprature ... - Nov 23, 2005 by MSK
Search the fine SMTnet Archives on "lead free component". ... - Nov 23, 2005 by davef
Are the components 100% tin plated? Thats what we are buying... - Nov 23, 2005 by
MKS, You do not need to reach a temp of 245C to form a joi... - Nov 29, 2005 by