What does MSL 4 on a component package means?

Ian CCY

#18542

What does MSL 4 on a component package means? | 3 January, 2002

Hi,

I am trying to write SOP about the baking requirement of some CSP and uBGA components, the label on the packing said its usable within 72 hours and follow the MSL 4 condition, what does the MSL means? is it Material Safety Level? Has anything to do with the baking condition? Where can I get information (Free) about the baking standard of SMT component?

Thanks

reply »

Ian CCY

#18543

What does MSL 4 on a component package means? | 3 January, 2002

Hi,

I am trying to write SOP about the baking requirement of some CSP and uBGA components, the label on the packing said its usable within 72 hours and follow the MSL 4 condition, what does the MSL means? is it Material Safety Level? Has anything to do with the baking condition? Where can I get information (Free) about the baking standard of SMT component?

Thanks

reply »

Scott Davies

#18546

What does MSL 4 on a component package means? | 3 January, 2002

MSL is "Moisture Sensitivity Level", and you should be able to find information on the websites of individual component manufacturers. For example, take a look at Infineon;

http://www.infineon.com/greenproduct/msl_classification1.htm

reply »

#18549

What does MSL 4 on a component package means? | 3 January, 2002

In addition to a previous poster's comments, you many want to understand moisture sensitive components better. Start with: * J-STD-020 and J-STD-033. Download them here: http://www.jedec.org/download/default.cfm

* �Moisture Sensitive Components� R Roland, SMT Magazine, 10/00, p.26, 28

reply »

#18556

What does MSL 4 on a component package means? | 3 January, 2002

I know fmonette has a MSD audit check list. Maybe when he posts, he'll give us a MSD control procedure aimed at operations types.

reply »

Ian CCY

#18560

What does MSL 4 on a component package means? | 3 January, 2002

Thanks guys, it's very helpful.

reply »

fmonette

#18572

What does MSL 4 on a component package means? | 4 January, 2002

As Dave mentioned we have put together a MSD audit checklist to insure that your internal procedure is complete and in line with J-STD-033.

It's a free download at http://www.cogiscan.com, click on Moisture Sensitive Devices to access the MSD Knowledge Base and then select MSD Audit Checklist.

I hope it's helpful.

Francois Monette Cogiscan Inc. Tel : 450-534-2644 E-mail : fmonette@cogiscan.com