BGA testing on the Agilent HP5DX x-ray System

squirera

#2783

BGA testing on the Agilent HP5DX x-ray System | 11 October, 2000

Has anyone had any success in finding open circuits (i.e. ball present but not soldered to PCB) under collapsible BGA's using an Agilent HP5DX x-ray tester and the BGA2 algorithm? Can anyone recommend an elongated pad design which produces the necessary difference in good/bad joint appearance to find opens but avoid false calls?