Issues with Immersion silver | 11 August, 2017

I am having issues with this. I am having excess plating on my pcb board and i want to know if this is a ICP Class 1-3 Issue.

1. Excess Plating 2. Dark Vias

Thank you

Attachments:

reply »

#78672

Issues with Immersion silver | 11 August, 2017

Hi Adonys, What's ICP 1-3? Do you mean IPC?

1. Excess Plating- no excess, but filled with something which generated in the process of copper plating.

2. Dark Vias - it's oxidized.

and the solder mask printing is not aligned. The board is failed. Maybe you can ask your supplier to issue an 8D reports for you.

by the way, I recommend http://www.madpcb.com, which is a professional pcb manufacturing, assembly and design provider.

reply »

#78773

Issues with Immersion silver | 31 August, 2017

Hello ALL Good day , it is Amalia from HX Circuit Technology Co.,Ltd in China, we are a prefessional PCB factory with many years. We are focusing on quick lead time for PCB with good service . please contact with me now ,thanks Email: amalia@hx-circuit.com Skype: amalia.zeng www.hx-circuit.com