Is it normal for *flux to stuck on the ricocel?

Views: 4277

#78406

Is it normal for flux to stuck on the ricocel's pallet? | 14 July, 2017

#78415

Is it normal for flux to stuck on the ricocel's pallet? | 14 July, 2017

How to clean Durostone wave solder pallet?

Add date:2016-1-13 Hits:657 Print Back

Ultrasonic machines are often used to clean the pallets. This machine is suitable to eliminate the wax, the oil and other stains. With high efficiency, excellent cleaning performance, it is very suitable for electroplating, hardware, electronics, light industry, mechanical industry, etc. People usually clean the pallet with water, neutral cleaning agent is also OK. Do not clean with strong acid or alkali. Never use alcohol to clean the wave solder pallet because Durostone is sensitive to alcohol. [Prior Plastic Co.,LTD.]

reply »


Tim

#78424

Is it normal for flux to stuck on the ricocel's pallet? | 17 July, 2017

We run our wave pallets through a batch was with chemistry and DI water, they do not come out 100% but they are much better than no washing at all. Water Soluble fluxes come off fairly easily. No clean fluxes are a pain to get off and I haven't been able to get the pallets to look clean but I can tell that the flux is mostly washed off.

Ricocel hasn't caught on much in the US yet, there is only one pallet supplier that I am aware of who uses it, Stentech. I would recommend contacting them and seeing if they have any washing recommendations or try contacting your flux supplier for wash recommendations.