HEllo all,

I changed a THERMOCOUPLE on my soldering pot. Now when I start the machine, pot shows 80C but it is over 300C. Any thoughts?

reply »

#76814

ACE KISS103 thermocouple calibration | 29 December, 2016

If you are in US, contact Dave at ACE. Their tech support is excellent.

reply »

#76815

ACE KISS103 thermocouple calibration | 29 December, 2016

mount you are off would seem a little large for a mis-calibration!

sarason

reply »

#76823

ACE KISS103 thermocouple calibration | 30 December, 2016

Is it the correct type of thermocouple? If it is designed for a K type and you put a J or T the reading will be lower. Also a bad connection can give a lower reading.

reply »

#76825

ACE KISS103 thermocouple calibration | 30 December, 2016

Thank you all. It was a bad connection. Everything is running fine. Happy new year to everyone! Emil