Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7227
Hello Folks, I am getting a Passaat SMRO-0406 reflow mach... - Dec 09, 2014 by Sreejith
Thanks for your reply!! But i dont understand the 300 degree... - Dec 10, 2014 by Sreejith
The 300 degrees is the temperature as measured at the sensor... - Dec 10, 2014 by JimPat
Hello, yes you are absolutely correct. I agree with your ... - Dec 10, 2014 by Sreejith
The longer the oven, the better. You will have much more cap... - Dec 11, 2014 by Evtimov
Hello Sir, Thanks for your reply. i just got a mail from ... - Dec 11, 2014 by Sreejith
ALso, coming to the convection the DIMA service group said :... - Dec 11, 2014 by Sreejith
Hello, So in short, i wanted to know.. for 8 zones i gues... - Dec 11, 2014 by Sreejith
If you have a chance ask them to bring in one of your produc... - Dec 11, 2014 by Evtimov
why all people speak only the temperatur? the speed convoyor... - Dec 22, 2014 by ben
What do you mean by solder in ROHS. Can you please explain m... - Dec 22, 2014 by Sreejith
Hello, Also I wanted to tell you. I decided to go with a ... - Dec 22, 2014 by Sreejith
Sounds like your volumes are pretty low. Pick and Place is ... - Dec 23, 2014 by JimPat