Hello, We are facing solderability issues on a particular... - Oct 27, 2014 by R
Rather than asking why, maybe the better response is to reje... - Oct 30, 2014 by Hegemon
Why soldering issues? I'd guess the nickel is corroded. It i... - Oct 30, 2014 by davef