Good day all, I wanted to get a quick poll from the folks running SAC305 in their selective soldering equipment.
How are final results? How repeatable is the process, any machine related failures? pumps? nozzles? etc...
I am just looking to get a feel from all of you in order to see how the industry is handling lead free solderability using selective soldering.
I appreciate your time and responses.