Heavy BGA Inspection

#6954

Heavy BGA Inspection | 18 June, 2001

We are assembling BGA [Texas Instruments (TMS320C6201)] that has metal slugs in the packaging that act as heat sinks. What are your recommendations for inspecting the solder connections on such devices?

This message was posted Add this forum to your site! Click to learn more. the OnBoard Forums

reply »

Gil Zweig

#6974

Heavy BGA Inspection | 19 June, 2001

When x-ray inspecting BGA packages with metal heat spreaders tube voltages greater than those used for Plastic BGAs must be used. It must be recognized, however, that the tube votage required will depend on the particular sensitivity of the x-ray camera employed. A commercial CsI image intensifier may require a tube operating at 100 kV whereas a high sensitivity x-ray camera will only require 70 kV to get comparable or better x-ray image.

This message was posted Add this forum to your site! Click to learn more. the OnBoard Forums

reply »