Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Setting limits in Solder Paste Inspection

Views: 4497

#66196

Setting limits in Solder Paste Inspection | 21 April, 2012

I am using different equipements for SPI such as Koh Young and Cyber Optics machines. I am looking for implementing a general procedure (SWP) for setting LSL's and USL's on the products on which the customer does not specify any limits on the solder deposition.

On most machines (Koh Young) i currently use an "SPC Plus" version software for 3D inspection as follows:

1. run a test lot of 10 PCBs on screen printing with printing parameters (squeegee speed/pressure, snap-off speed/distance etc) in concordance with PCB dimensions.

2. start from a group of limits in SPI selected according to the stencil thickness (ie: for 100um stencil thickness i use lower limit of 70um and an upper limit of 170um). I use these limits on the whole stencil, for all the apertures. I only ise different USL and LSL for aperture groups in case of STEP UP/DOWN stencils.

3. on SPI program (particularly Koh Young's SPC Plus), i look for the height histogram. here i can see my lowest and highest limits for the test run. Considering the test run stable enough, i could go +/- 10um from LSL and USL and choose those values as my valid mass production limits for paste deposit height.

All these work well in the field, but i don't currently have a SWP on chosing these limits and i can't find anything else on the internet about this.

My problem is: is there a standard to choose these limits? +/- 10um over and under test run limits is OK, but why not 15um, if all PCBAs are PASS VIAR (visual inspection after reflow)?
Is there any formula on calculating the limits?

reply »

#66229

Setting limits in Solder Paste Inspection | 27 April, 2012

I have worked with Chrys Shea for a number of years. She has written a few white papers on SPI that may be beneficial to you. Here is a link to her website; http://sheaengineeringservices.design.officelive.com/default.aspx

reply »

#66365

Setting limits in Solder Paste Inspection | 18 May, 2012

Dear brotakul ,
Please let me know if the white paper is traced as the link given is not active .

Thanks
Vikas

reply »

#66367

Setting limits in Solder Paste Inspection | 18 May, 2012

> Dear brotakul , Please let me know if the white
> paper is traced as the link given is not active
> .
>
> Thanks Vikas

hello,
Chrys recently updated her website; here is the new link http://www.sheaengineering.com/wpapers.html

reply »

#66369

Setting limits in Solder Paste Inspection | 18 May, 2012

Hello CAPSE,

The link you posted is not available.

reply »

#66372

Setting limits in Solder Paste Inspection | 18 May, 2012

#66375

Setting limits in Solder Paste Inspection | 19 May, 2012

Thank you, interesting reading.

reply »

#66378

Setting limits in Solder Paste Inspection | 20 May, 2012

Hi ,
Thanks for the link and could understand the limit setting .

Regards
Vikas

reply »

#66388

Setting limits in Solder Paste Inspection | 21 May, 2012

hi,
the link works for me
here is the URL for the web site;
http://www.sheaengineering.com good luck

reply »