Repair Units | 26 January, 2012

Sir i need someones expertise on my problem.
We are running repair unit which we conduct FFC removal in this process we are encountering big problem by whick we lessen solder deposit on our PCB..
1. Can you give me some idea on what way can we put additional solder on our PCB?
2. Spec's 57 pins 0.5mm pitch

We already reprocess by again Solder paste printing and refolw..

NEED your expertise on this

reply »

#65788

Repair Units | 26 January, 2012

Here's what we hear you saying:
* Trying to repair a printed circuit board assembly
* There's a problem replacing a 57 pin, 20 thou connector
* Can't get enough solder paste on the connector leads
* Printing paste, replacing the connector, then reflowing the assembly

If so, try either:
* Open up the apertures of your stencil ... OR
* Use a thicker stencil ... OR
* In addition to what you're presently doing, use a manual paste dispense gun to lay a line of paste over the connector leads. Then reflow

If not, give us more detail

reply »

#65908

Repair Units | 24 February, 2012

Hi, guys, this is jack from soppcb technolgy in shenzhen, we are a professioanl manufacturer of PCB and PCBA, including single sided pcb, double boards, multilayer boards, HDI, aluminum led boards and so on, if any needs, pls contact me here or my address: soppcbtech at gmail dot com

reply »

Used PCB Equipment  - Europe
SMT Reflow Soldering Oven
Now Online

455
Visitors

2
Members

Featured Companies
 

SRT Micra, High Through-put rework station