Is there a different thickness of screens we should be usi... - Jan 23, 2012 by gaz
Area Ratio [PCB Assembly Guidelines for 0.4mm Package-On-Pac... - Jan 23, 2012 by davef
If you failed math like I did. A 0.005 inch stencil would wo... - Jan 24, 2012 by KaHrpr
We are using 6 mil screens, and these boards have 0603,SOT23... - Jan 25, 2012 by gaz
Your uising 6 mil thick screen on 0603 and sot-23 and you t... - Jan 25, 2012 by WRONGWAY
A few years ago a lot of stencils were 6 mill and 7 mills an... - Jan 25, 2012 by KaHrpr
We're in the high rel market and use a lot of 5 mil stencils... - Jan 27, 2012 by ScottE
Thanks very much everyone. I'll try out a 5mil and se... - Feb 01, 2012 by gaz
> Thanks very much everyone. > > I'll try out a ... - Feb 03, 2012 by aci
By changing paste and making a better profile, it seems like... - Feb 06, 2012 by gaz
What is the percent solids of the paste you are using? ... - Feb 14, 2012 by isd.jww
Is that the "general metal loading" spec? We are usin... - Feb 16, 2012 by gaz