I am trying to rework FP4531 underfill. Some of the underfil... - Jul 26, 2011 by indyc
indyc
#64702
FP4531 underfill rework | 26 July, 2011
I am trying to rework FP4531 underfill. Some of the underfill flowed to adjacent capacitor and resistor. Even though the datasheet says that it is non-reworkable, has anyone tried reworking / removing excess underfill?
Any information would be help.