Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6937
Dear All I need to check the solder paste volume inside t... - Oct 06, 2010 by Jacki
> Dear All > > I need to check the solder paste ... - Oct 13, 2010 by Florin Costache
Thanks Florin Yes, it is difficult to find a AXI machine fo... - Oct 13, 2010 by Jacki
hi i dont know this 2 systems, i work with %DX frm Agilen... - Oct 14, 2010 by Florin Costache
Thanks Florin Yes, XD7800NT950 is capable to inspect our su... - Oct 17, 2010 by Jacki
Hi Jacki, My name is Sandor and we are DAGE representativ... - Oct 18, 2010 by Sandor Babos
Hi Sandor I just reached the local DAGE guy,CH Liu. Thank... - Oct 21, 2010 by Jacki