Cobalt in leadfree solder alloys?

Views: 311
Cobalt in leadfree solder alloys? Steve   10/23/09
Cobalt in leadfree solder alloys? davef   10/26/09

Email This Page to a Friend


TopPreviousNextPrintReply

Date: October 23, 2009 02:20 PM
Author: Steve  
Subject: Cobalt in leadfree solder alloys?

We offer SN100C solder alloys. I was asked about SN100E which is tin/copper and cobalt. Anyone know anything about the cobalt and it's pros and cons in soldering process?

(http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=60170)


    TopPreviousNextPrintReply

    Date: October 26, 2009 03:38 PM
    Author: davef  
    Subject: Cobalt in leadfree solder alloys?

    We believe that some suppliers replace nickel with cobalt in SN100 to product a shinier, less grainy, more attractive lead-free solder connection.

    SN100E sales-types like the idea that it is available in paste, bar stock, and other forms; as compared with SN100C that is not available in as many forms.

    (http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=60188)








 
manufacturing software
 
 
 
 
 

Click here for text advertising info

    Back to the Top License Agreement       Privacy Policy       Contact Us    Copyright © SMTnet 1995-2009    Back to the Top