Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 9349
In the SMT “Gluing Process” we are using “Thermosetting Poly... - Sep 10, 2009 by eeeee
The adhesive should be a dielectric (insulator) by design, i... - Sep 10, 2009 by MikeS
Questions are: * Could it be that there's a difference betw... - Sep 10, 2009 by davef
Hi Davef & Mikes, Thanks for the response. I am agree with ... - Sep 18, 2009 by eeeee
First, we're not real concerned about gluing induced ESD dam... - Sep 21, 2009 by davef
Thnaks for the input. ... - Sep 22, 2009 by eeeee
> Second, ESD-stuff > IS very confusing. Largely bec... - Sep 22, 2009 by Stephen
Hi Stephen, Can you pl suggest what exactly needed for th... - Sep 22, 2009 by eeeee
I did see ESD issues years ago when we tried using a plastic... - Sep 23, 2009 by ScottE
Can you pl let us know what was the ESD sensitivity level of... - Sep 24, 2009 by eeeee
We're in the high reliability market and build to IPC Class ... - Sep 24, 2009 by ScottE