Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2598
I read somewhere there is a thermal measure that takes into ... - Aug 27, 2008 by blnorman
Td - is the degradation temperature for a laminate (board), ... - Aug 27, 2008 by Vlad
I know, but somewhere I read about an equation or relationsh... - Aug 27, 2008 by blnorman
While you're waiting for others to reply, here are a couple ... - Aug 27, 2008 by davef
Yep, that is probably the one in the Werner's paper. Vlad... - Aug 27, 2008 by Vlad
BINGO. I knew there was some relationship between the 2, th... - Aug 28, 2008 by blnorman