Does anyone have any experience with DeFelsko Corporation th... - Jul 20, 2007 by MGL
From NASA document: Conformal coating thickness shall be de... - Jul 23, 2007 by PeteC
NASA-STD-8739.1, 10.2.3 Thickness Measurements. Thickness me... - Jul 23, 2007 by davef
We run a small piece of FR4 with a "thickness test" pattern ... - Jul 23, 2007 by jdumont
It's it curious that NASA requires 'Thickness measurements s... - Jul 23, 2007 by davef
Josh: Do you measure the thickness of the coupon prior to co... - Jul 23, 2007 by davef
We have not had the best of luck with wet film. I agree on y... - Jul 23, 2007 by MGL
We have used many ways of measuring but all are either messy... - Jul 23, 2007 by MGL
We know nothing of DeFelsko, but do understand how they dist... - Jul 23, 2007 by davef
We just measure the coupon before and after. We are always b... - Jul 24, 2007 by jdumont